General information
Country
India
Publish Date
February 22, 2022
Description of the case
Using stud welding instead of countersink drilling and CSK Bolts. Increases the total lifetime of liners. Earlier in CSK bolts max usage of liner was up to 10-12 mm. Now usage up to 3-4 mm.
-
0 – 250 °C / 32 – 480 °F
-
10 – 300 mm / 0.4 – 12.0 "
-
Coal
New solution
New solution
Hardox® 500
Thickness
25
Service life
3 years
Key success factors
Improved service life
140%
Lower initial cost
No drilling
Lower lifetime costs
40%